Engineering Materials Which of the following property is desirable in parts subjected to shock and impact loads? Brittleness Stiffness Toughness Strength Brittleness Stiffness Toughness Strength ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials The machinability of steel is increased by Phosphorous, lead and sulphur Phosphorous and aluminium Silicon and sulphur Sulphur, graphite and aluminium Phosphorous, lead and sulphur Phosphorous and aluminium Silicon and sulphur Sulphur, graphite and aluminium ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials Corrosion resistance of steel is increased by addition of Chromium and nickel Tungsten, molybdenum, vanadium, chromium Sulphur, phosphorus, lead Vanadium, aluminium Chromium and nickel Tungsten, molybdenum, vanadium, chromium Sulphur, phosphorus, lead Vanadium, aluminium ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials Iron-carbon alloys containing carbon ________ 4.3% are known as hyper-eutectic cast irons. More than Less than Equal to None of these More than Less than Equal to None of these ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials Points of arrest for iron correspond to There is nothing like points of arrest Stages at which properties do not change with increase in temperature Stages at which allotropic forms change Stages at which further heating does not increase temperature for some time There is nothing like points of arrest Stages at which properties do not change with increase in temperature Stages at which allotropic forms change Stages at which further heating does not increase temperature for some time ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials According to Indian standard specifications, plain carbon steel designated by 40 C8 means that the carbon content is 0.0004 0.6 to 0.8% 0.4 to 0.6% 0.35 to 0.45% 0.0004 0.6 to 0.8% 0.4 to 0.6% 0.35 to 0.45% ANSWER DOWNLOAD EXAMIANS APP