Engineering Materials Tungsten in high speed steel provides Toughness Sharp cutting edge Wear resistance Hot hardness Toughness Sharp cutting edge Wear resistance Hot hardness ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials Induction hardening is basically a Carburising process Surface hardening process None of these Core hardening process Carburising process Surface hardening process None of these Core hardening process ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials The ability of a material to absorb energy in the plastic range is called Fatigue strength Resilience Creep Toughness Fatigue strength Resilience Creep Toughness ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials Gamma-iron occurs between the temperature ranges of 400°C to 600°C 900°C to 1400°C 600°C to 900°C 1400°C to 1530°C 400°C to 600°C 900°C to 1400°C 600°C to 900°C 1400°C to 1530°C ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials White metal contains 63 to 67% nickel and 30% copper Alloy of tin, lead and cadmium 88% copper and 10% tin and rest zinc Silver and chromium 63 to 67% nickel and 30% copper Alloy of tin, lead and cadmium 88% copper and 10% tin and rest zinc Silver and chromium ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials The machinability of aluminium increases when _________ is added to aluminium. Silicon Lead and bismuth Copper Magnesium Silicon Lead and bismuth Copper Magnesium ANSWER DOWNLOAD EXAMIANS APP