Engineering Materials The charge of the blast furnace consists of Calcined ore (1 part), coke (8 parts) and limestone (4 parts) Calcined ore (4 parts), coke (1 part) and limestone (8 parts) Calcined ore, coke and limestone all in equal parts Calcined ore (8 parts), coke (4 parts) and limestone (1 part) Calcined ore (1 part), coke (8 parts) and limestone (4 parts) Calcined ore (4 parts), coke (1 part) and limestone (8 parts) Calcined ore, coke and limestone all in equal parts Calcined ore (8 parts), coke (4 parts) and limestone (1 part) ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials The brown smoke during the operation of a Bessemer converter indicates that the Air is burning out silicon and manganese The brown smoke does not occur during the operation of a Bessemer converter Silicon and manganese has burnt and carbon has started oxidizing The converter must be titled to remove the contents of the converter Air is burning out silicon and manganese The brown smoke does not occur during the operation of a Bessemer converter Silicon and manganese has burnt and carbon has started oxidizing The converter must be titled to remove the contents of the converter ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials In full annealing, the hypo eutectoid steel is heated from 30°C to 50°C above the upper critical temperature and then cooled Any one of these Slowly in the furnace Suddenly in a suitable cooling medium In still air Any one of these Slowly in the furnace Suddenly in a suitable cooling medium In still air ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials Tungsten in steel Refines grain size and produces less tendency to carburisation, improves corrosion and heat resistant properties Improves wear resistance, cutting ability and toughness Gives ductility, toughness, tensile strength and anti-corrosion properties Improves cutting ability and reduces hardenability Refines grain size and produces less tendency to carburisation, improves corrosion and heat resistant properties Improves wear resistance, cutting ability and toughness Gives ductility, toughness, tensile strength and anti-corrosion properties Improves cutting ability and reduces hardenability ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials Blast furnace produces following by reduction of iron ore Wrought iron Malleable iron Cast iron Pig iron Wrought iron Malleable iron Cast iron Pig iron ANSWER DOWNLOAD EXAMIANS APP
Engineering Materials Which of the following element results in presence of free graphite in C.I.? Sulphur Manganese Carbon Silicon Sulphur Manganese Carbon Silicon ANSWER DOWNLOAD EXAMIANS APP