Engineering Materials
White cast iron

Is also known as chilled cast iron and is obtained by cooling rapidly. It is almost unmachinable
Is produced by annealing process. It is soft, tough and easily machined metal
Is produced by small additions of magnesium (or creium) in the ladle. Graphite is in nodular or spheroidal form and is well dispersed throughout the material
Contains 1.7 to 3.5% carbon in Free State and is obtained by the slow cooling of molten cast iron

ANSWER DOWNLOAD EXAMIANS APP

Engineering Materials
In a hardening process, the hypo-eutectoid steel is

Heated from 30°C to 50°C above the upper critical temperature and then cooled suddenly in a suitable cooling medium
Heated from 30°C to 50°C above the upper critical temperature and then cooled slowly in the furnace
Heated below or closes to the lower critical temperature and then cooled slowly
Heated from 30°C to 50°C above the upper critical temperature and then cooled in still air

ANSWER DOWNLOAD EXAMIANS APP

Engineering Materials
Dow metal contains

94% aluminium, 4% copper and 0.5% Mn, Mg, Si and Fe
90% aluminium and 90% copper
90% magnesium and 9% aluminium with some copper
92.5% aluminium and, 4% copper, 2% nickel and 1.5% Mg

ANSWER DOWNLOAD EXAMIANS APP