Refractory Technology With increase in the density of silica refractories, its Spalling resistance reduces Neither A nor B Both A & B Resistance to slag attack increases Spalling resistance reduces Neither A nor B Both A & B Resistance to slag attack increases ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Insulating refractories should have High porosity Low thermal conductivity Both A & B Neither A nor B High porosity Low thermal conductivity Both A & B Neither A nor B ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Firing of refractory brick is done to Dehydrate the dried refractory All of these Develop stable mineral forms in them Form ceramic bonds necessary for development of high crushing strength in the finished product Dehydrate the dried refractory All of these Develop stable mineral forms in them Form ceramic bonds necessary for development of high crushing strength in the finished product ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Maximum apparent porosity of magnesite bricks is about __________ percent. 44 8 24 58 44 8 24 58 ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Cold crushing strength of ordinary fireclay brick is about 950 kg/cm² . On exposure to a temperature of about 1500°C, its crushing strength may come down to as low as __________ kg/cm² . 450 150 250 65 450 150 250 65 ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Periclase is Amorphous magnesite Crystalline form of MgO MgCO₃ ZrSO₄ Amorphous magnesite Crystalline form of MgO MgCO₃ ZrSO₄ ANSWER DOWNLOAD EXAMIANS APP