Materials and Construction

Materials and Construction
Which of the following undergoes granular fracture?

Wrought iron
None of these
Cast iron
Steel

ANSWER DOWNLOAD EXAMIANS APP

Materials and Construction
In a plate type heat exchanger, heat transfer plates are never made of

Cast iron
Hastealloy C
Titanium
Stainless steel

ANSWER DOWNLOAD EXAMIANS APP

Materials and Construction
Constantan is an alloy of

Fe (80%) & Ni (20%)
Pt (95%) & Rh (10%)
Cu (55%) & Ni (45%)
Cu (55%) & Sn (45%)

ANSWER DOWNLOAD EXAMIANS APP

Materials and Construction
__________ is added in stainless steel to prevent inter crystal corrosion.

Vanadium
Nickel
Niobium
Chromium

ANSWER DOWNLOAD EXAMIANS APP

Materials and Construction
Molybdenum steels containing 0.15 to 0.40% molybdenum

Are prone to temper brittleness
Do not contain nickel or chromium or both
Are used for automobile parts like gears, axle, shaft, bearings etc
Have very poor fatigue resistance

ANSWER DOWNLOAD EXAMIANS APP

Materials and Construction
Addition of nickel to copper improves its

Hardness
Strength
Machinability
Ductility

ANSWER DOWNLOAD EXAMIANS APP
MORE MCQ ON Materials and Construction

DOWNLOAD APP

  • APPLE
    from app store
  • ANDROID
    from play store

SEARCH

LOGIN HERE


  • GOOGLE

FIND US

  • 1.70K
    FOLLOW US
  • EXAMIANSSTUDY FOR YOUR DREAMS.
  • SUPPORT :SUPPORT EMAIL ACCOUNT : examians@yahoo.com

OTHER WEBSITES

  • GUJARATI MCQ
  • ACCOUNTIANS

QUICK LINKS

  • HOME
  • QUIZ
  • PRIVACY POLICY
  • DISCLAIMER
  • TERMS & CONDITIONS
  • CONTACT US
↑