Polymer Technology Temperature and gage pressure maintained during the manufacture of hot SBR (styrene butediene rubber) are 50°C and 1 kgf/cm² 250°C and 10 kgf/cm² 250°C and 1 kgf/cm² 50°C and 3 - 4 kg/cm² 50°C and 1 kgf/cm² 250°C and 10 kgf/cm² 250°C and 1 kgf/cm² 50°C and 3 - 4 kg/cm² ANSWER DOWNLOAD EXAMIANS APP
Polymer Technology Phosphates (e.g., triceresyl, tributyl, tetrabutyl, tripheyl etc.) are added to polymers to act as Transparency improver Hardeners Plasticisers Anti-shrinkage agents Transparency improver Hardeners Plasticisers Anti-shrinkage agents ANSWER DOWNLOAD EXAMIANS APP
Polymer Technology Crystallisation of polymers is an undesirable property. Crystallisation of celluloid is prevented by adding Camphor Nitro cellulose None of these Glycerol Camphor Nitro cellulose None of these Glycerol ANSWER DOWNLOAD EXAMIANS APP
Polymer Technology Automobile steering wheels are normally made of Cellulose acetate PVC High density polythene Cellulose nitrate Cellulose acetate PVC High density polythene Cellulose nitrate ANSWER DOWNLOAD EXAMIANS APP
Polymer Technology Mastication of rubber means Improving its curing rate Its softening A treatment to retard its deterioration due to oxidation Depression of its freezing point Improving its curing rate Its softening A treatment to retard its deterioration due to oxidation Depression of its freezing point ANSWER DOWNLOAD EXAMIANS APP
Polymer Technology A chain growth polymerisation reaction consists of three different types of reaction namely initiation reaction, propagation reaction & termination reaction. Chain growth polymerisation reaction is not involved in the manufacture of Siloxane elastomers Polyamides Vinyl polymers Urea-formaldehyde resins Siloxane elastomers Polyamides Vinyl polymers Urea-formaldehyde resins ANSWER DOWNLOAD EXAMIANS APP