Refractory Technology Refractoriness under load (RUL) of fireclay bricks (under a load of 2 kg/cm² ) is __________ °C. 1000 >1350 >2000 500 1000 >1350 >2000 500 ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Porosity is induced in insulating refractories by adding Calcium phosphate Powdered naphthalene All of these Ammonium chloride/sulphate Calcium phosphate Powdered naphthalene All of these Ammonium chloride/sulphate ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Refractory bricks having lower porosity have High insulating properties Greater strength Low thermal conductivity Low heat capacity High insulating properties Greater strength Low thermal conductivity Low heat capacity ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Cold crushing strength of ordinary fireclay brick is about 950 kg/cm² . On exposure to a temperature of about 1500°C, its crushing strength may come down to as low as __________ kg/cm² . 450 65 150 250 450 65 150 250 ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Which is the stable form of silica upto 1470°C ? Tridymite Cristobalite Quartz None of these Tridymite Cristobalite Quartz None of these ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Pyrometric cone equivalent (PCE) of a refractory is the measure of its Resistance to carbon monoxide attack Resistance to slag penetration Spalling resistance Fusion point Resistance to carbon monoxide attack Resistance to slag penetration Spalling resistance Fusion point ANSWER DOWNLOAD EXAMIANS APP