Engineering Materials
Tungsten in steel

Improves wear resistance, cutting ability and toughness
Refines grain size and produces less tendency to carburisation, improves corrosion and heat resistant properties
Gives ductility, toughness, tensile strength and anti-corrosion properties
Improves cutting ability and reduces hardenability

ANSWER DOWNLOAD EXAMIANS APP

Engineering Materials
In process annealing, the hypo eutectoid steel is

Heated from 30°C to 50°C above the upper critical temperature and then cooled slowly in the furnace
Heated below or closes to the lower critical temperature and then cooled slowly
Heated from 30°C to 50°C above the upper critical temperature and then cooled in still air
Heated from 30°C to 50°C above the upper critical temperature and then cooled suddenly in a suitable cooling medium

ANSWER DOWNLOAD EXAMIANS APP

Engineering Materials
Cobalt in steel

Gives ductility, toughness, tensile strength and anti corrosion property
Refines grain size and produces less tendency to carburisation, improve corrosion and heat resistant proper ties
Improves wear resistance, cutting ability and toughness
Improves cutting ability and reduce hardenability

ANSWER DOWNLOAD EXAMIANS APP