Electrolysis and Storage Batteries In order that a hydrometer may float vertically in electrolyte its C.G. should be lowered undisturbed raised displaced sideways lowered undisturbed raised displaced sideways ANSWER DOWNLOAD EXAMIANS APP
Electrolysis and Storage Batteries Ampere hour capacity of an industrial battery is based on ____ hours discharge rate. 24 8 10 12 24 8 10 12 ANSWER DOWNLOAD EXAMIANS APP
Electrolysis and Storage Batteries Charging a sulphated battery at high rate results in warping of plates damage to separators, cell caps covers and battery case due to excessive temperature boiling of electrolyte due to gassing All of the listed here warping of plates damage to separators, cell caps covers and battery case due to excessive temperature boiling of electrolyte due to gassing All of the listed here ANSWER DOWNLOAD EXAMIANS APP
Electrolysis and Storage Batteries Excessive formation of lead sulphate on the surface of the plates happens because of allowing a battery to stand in discharged condition for a long time persistent undercharging all of the listed here low level of electrolyte allowing a battery to stand in discharged condition for a long time persistent undercharging all of the listed here low level of electrolyte ANSWER DOWNLOAD EXAMIANS APP
Electrolysis and Storage Batteries Undercharging Increases the temperature Produces excessive gassing Increases specific gravity of the electrolyte Reduces specific gravity of the electrolyte Increases the temperature Produces excessive gassing Increases specific gravity of the electrolyte Reduces specific gravity of the electrolyte ANSWER DOWNLOAD EXAMIANS APP
Electrolysis and Storage Batteries During charging the specific gravity of the electrolyte of a lead-acid battery decreases remains the same increases none of the listed here decreases remains the same increases none of the listed here ANSWER DOWNLOAD EXAMIANS APP